Alloy |
Cu-DHP CW024A (Cu = 99.90% min. - P = 0.015 ÷ 0.040%) |
Physical state according to EN 1057 |
Annealed R220 |
Half-Hard R250 |
Hard R290 |
Unit tensile strength - R min. |
220 N/mm² |
250 N/mm² |
290 N/mm² |
Percentage elongation - A min. |
40% |
20 - 30% |
3% |
Total carbon |
C = 38 mg/m² according to standard EN 12735-1 |
Marking on tube |
EN 12735-1 diameter batch number |
Dimensions and tolerances |
According to standard EN 12735-1 |
Internal surface roughness |
RA - 1/10 micron |
Linear thermal expansion coefficient |
0.00168 mm/m °C |
Thermal conductivity at 20°C |
364 W/m · K |